In general terms, this occurs with air dried paints (1 part) where the surface dries quickly but the underlying paint takes much longer because it is sealed off from air by the surface skin. Heavy coats are an aggravating factor. Wrinkling is prevented by applying several thin coats with sufficient drying time between. Once wrinkling has occurred, the entire finish must be removed and started over. Trying to remedy what is already there will be an exercise in futility.
Paint choice can help. Two part (catalyzed) paints dry chemically through the entire thickness. Cobalt drier is an additive that acts as a drying accelerant in air dried oil based paints (1 part) but should not be considered an alternative to thin coats.