Quote:
Originally Posted by TimBSmith View Post
...Has anyone used 316/316L stainless nipple with the Moyer flange or SS nipple or connector to Moyer water injector? Have you noticed accelerated galvanic corrosion?
I have both in my hot section. Although I can't easily inspect it due to the wrapping, it has been in operation since 2011 and has over 1800 hours on it without showing any signs of leakage.

Quote:
Originally Posted by TimBSmith View Post
...I am planning to provide some additional surface rust protection using high temperature primer.
I am not sure that painting the SS parts is a good idea. Stainless rusts by a process called "Crevice Corrosion", which requires the absence of air to get started. Painting would seal off the surface, allowing saltwater to get under the paint at any scratch and begin corrosion.